Common defects in paint treatment method of atomic ash and bleeding

source:date:2015-6-10 9:51:07


After spraying paint, used in the area of atomic ash, the surface color change, often show the color around the light, especially light blue and green color silver paint is easy to appear this kind of phenomenon.


(1) cause

(1) the atomic ashes curing agent, curing agent of oxide bleaching results in uneven color pigment.

(2) the putty and poor quality.


(2) correction method

Atomic ash (1) with good quality, and with reference to the use of atomic ash that right mix ratio of putty and hardener.

(2) if the bleeding phenomenon has occurred, the surface should be polished lacquer layer and repainting, severe cases should be polished away putty coating and repair again.



清远雅克化工有限公司 @ All rights reserved 2015 | 粤ICP备06084242号 | The website construction:Qingyuan rubik's cube network
address:Qingyuan city, guangdong province high-tech development zone Silver light jia fu jia by 16 industrial zone tel:0763-3607328 email:yakoo@yakoo.com.cn

在线客服

树脂
点击这里给我发消息
原子灰
点击这里给我发消息
工业漆
点击这里给我发消息
点击这里给我发消息